Surface Finishing: Advantages & Disadvantages
Why do we need a surface finish?
Surface finish is necessary for 2 key reasons:
- To prevent oxidation of exposed copper surfaces which would lead to poor solderability/reliability.
- To provide a reliable, solderable surface which acts as the connection between the PCB and the components.
Advantages and disadvantages
|
HASL |
OSP |
ENIG |
| Advantages |
- Excellent Solderability
- Low Cost
- Long Shelf Life
- Long industry experience / well-known finish
|
- Good planarity for surface mount and HDI
- Simple Process
- Low Cost
- Environmentally Friendly
|
- Flat Surface
- Long shelf life
- Excellent oxidation resistance and wetting properties
- Robust for multiple thermal cycles
- Ideal for fine pitch surface mount, BGA ETC…
|
| Disadvantages |
- Poor surface planarity and variation
- Extremely aggresive thermal shock and stresses on PCB
- Not Recommended for HDI products (no BGA, SMD)
|
- 6 Months or less shelf life
- Very sensitive to handling poor Solderability
- Usually requires aggresive flux / cleaning
- Issues with multiple assembly process step
|
- Expensive finish
- nickel corrosion / black pad
- complicated process
- Possible damage from electrical test and routing
|
Advantages and disadvantages
|
Immersion Silver |
Immersion Tin |
Electrolytic Nickel Gold
(Hard or Soft Bondable) |
| Advantages |
- Metallic Finish
- Very flat and planar surface
- Ideal for surface mount, BGA ETC…
|
- Flat surface
- fine grain and non-porous
|
- Can be applied in varying thicknesses
- Gold can be deposited in varying degrees of hardness depending on application
- 12 month shelf life
- good planarity
|
| Disadvantages |
- Sensitive to handling and packaging
- Possible damage from electrical test
- Limited shelf life (up to 12 months)
- Creep-corrosion
|
- 6 month shelf life
- upleasant chemistry with carcinogenic substance – Thiourea
- Handling issues
- Potential for tin whisker growth over time – short circuits
|
- Undercut of copper under nickel creates overhang and potential for flaking/shorts
- Expensive
|